Before & After Pipe Stem Deoxidizer and Fine and Extra Fine Polishes from buzai232's blog

Before & After Pipe Stem Deoxidizer and Fine and Extra Fine Polishes

Before I write a review of a product I commit myself to use it for at least a month on a variety of pipes that have the issues that it was designed to address. I figure that during this time I will either have good reason to reject it as not helpful or to be sold on it enough to add it to my normal pipe cleaning and restoration routine. I clean and refurbish quite a few pipes each month so a product that says it will do such and such a job better deliver or it goes into the waste can. I don’t have time for products that do what I already can do at least as well with what I have.Get more news about Acrylic Deoxidizer,you can vist our website!

So committed to giving the product a solid trial, I purchased a small bottle of the Pipe Stem Deoxidizer and a jar of each of the Polishes. I have to admit up front, that I purchased this product with low expectations. I fully expected it to fit the “I already have products that work this well” category or that it would not deliver at all. I have tried a lot of stem polishes and deoxidizers over the years and they sit in the drawer wasting away with neglect. I was dubious from the start with this one, but I was committed to varying my routine and trying it out.

I begin the review with a little background information on the product, the cost and a few added instructions. I include the latter category because I missed it the first time around and it almost caused me to miss out on using a product that works well.

Background

I became acquainted with the Before & After Pipe Stem Deoxidizer and Polishes from posts on Facebook. For several months, I followed the work of Mark Hoover on the Gentlemen’s Pipe Smoking Society group on Facebook. He posted some of the most oxidized stems and then posted what they looked like after he used a product that he developed originally for working on pens. I kept reading and looking and just did not bite. I have used many different people’s concoctions for removing oxidation from stems and really none of them actually did it any better than a lot of elbow grease and time. But there was something about the work he posted that caught my eye and kept me looking. I think the thing that hooked me was that he did a stem and his product cleaned up the stem and left the logo stamp intact. It did no harm the paint in the stamp and it did not need any protection on the stamp before the product was used.
I wrote Mark using Facebook Messenger and asked him about the product and its availability in Canada. He wrote back almost immediately and said that he had shipped quite a few bottles to Canada and had no difficulties with it. He had some available in two different sizes – 8 ounces and 16 ounces. He said that each bottle had slightly more than the label said as he overfilled them. He said that each bottle would do quite a few stems depending on the level of oxidation. He figures that an 8 ounce bottle will do at least 15-20 stems heavily oxidized stems. The less oxidation on the stems the greater the number of stems that can be done.

The cost of the product was $20 USD for an 8 ounce bottle and $40 USD for a 16 ounce bottle. He also sold a Fine and an Extra Fine Pipe Stem Polish. The price of each jar of the polish was $12 USD. He said that a jar of polish can take care of between 40 and 50 stems. The product is label as Hard Rubber Deoxidizer on the site but it is the same thing. We wrote a few messages back and forth and we struck a deal. I quickly made a payment via PayPal and the product was on its way to Vancouver.